Yield strength: ≥ 355MPa
Tensile strength: 490MPa -630MPa
Elongation rate: ≥ 18%
St52-3 heat treatment status:
Delivery in states such as annealing, normalizing rolling, hot rolling, controlled rolling, normalizing, TMCP, etc
ST52-3 Chemical composition:
C carbon - ≤ 0.20% Si silicon - ≤ 0.50% Mn manganese - ≤ 1.98% P phosphorus - ≤ 0.040%
S sulfur - ≤ 0.040%