Why is it easy to block the water outlet during the continuous casting process of special steel

   Because special steel contains a lot of alloy elements, especially more active metal elements. Such as Al, Ti, Cr, Ni, Mn, etc. These elements can easily combine with O and N to form complex inclusions such as A1203, Ti02, Ti (CN), (Cr-A1) 203, and (Mn Ti) 204. This not only results in poor fluidity of the molten steel, but also makes it easy to block the nozzle during the pouring process.



评论

此博客中的热门博文

Japanese Standard (1)

National Standard Properties of 304 Stainless Steel Plate

Similarities and Differences in Performance between N08367 and N08926